NSN: 3439-00-201-9119 | Model: MILE19933

A coated or uncoated filler metal or an uncoated nonfiller material in wire or solid rod form. It is used in welding where the fusing or melting heat is supplied through the medium of an electric arc wherein the rod serves as carrier of the electric current. For a collection of welding electrodes, see welding electrode set. Excludes electrode, cutting, solid.

NSN Properties and Flags
NATO Stock Number
3439-00-201-9119
DEMIL
NO
Outside Diameter
0.062 inches
Current Type
Dc
Polarity Characteristic
Straight
Filler Metal Chemical Composition In Percent
9.00 nickel first element and 11.00 nickel first element
Criticality Code Justification
Zzzx
Material
Chromium and nickel and steel
Material Specification
Mil-e-19933, type mil-308 military specification single material response
Nondefinitive Specification/std Data
1a class and mil-308 type
Departure From Cited Designator
Material controlled iaw navsea 0948-lp-045-7010 material control standard for level i items

Pricing and Availability

Send us a request for quote using the form below. Our team will contact you with an up to date pricing and availability quote ASAP.

Qty:
Email Address:
Phone Number:
Your name:
Company:
Privacy    Terms

Certified Quality Assurance  Quality check icon

  •   ISO 9001:2015 + AS9120B
  •   Counterfeit Parts Prevention
  •   100% Product Inspections
  •   7 Year Record Retention
  •   On Time Delivery
  •   HAZMAT Certified
  •   Worldwide Shipping

NSN 3439-00-201-9119 Datasheet

Supply Class (FSC):
Brazing Supplies And Accessories Soldering Miscellaneous Welding
Cross Reference:
  • MILE19933
  • MILE19933L1
  • MIL-E-19933
  • MIL-E-9933MIL308CL1A1-16
  • MIL-E-19933L1
  • MIL-E-9933MIL308CL1A1-16L1
Cage Codes:
  • Military Specifications (CAGE 81349)
  • Naval Inventory Control Point (CAGE 03950)
Identification:
HMIC

Y - Indicates information is in the hazardous materials information resource system (hmirs).

PMIC

A - Item does not contain precious metal.

ADPE

- Represents items with no adp components

CRITL

- The item is a non-aviation critical safety item (csi) whose failure will result in serious damage to equipment or serious injury or death to personnel.

Freight Information:
  • NMFC:

    104390 - Bars, rods or wire, welding

  • WCC:

    746 - Welding equipment and soldering supplies

  • SHC:

    9 - Other or no special handling required (sh)

  • ADC:

    A - Shipment is not a consolidation and does not exceed 84 inches in any dimension.

  • ACC:

    B - Construction materials: includes paint and related materials, prefabricated building, wood products, metal and composition mater

  • LTL:

    W - Rating variable

  • TCC:

    Z - No special type of cargo code applicable

NSN Management Codes:
  • SOS
    Nrp
  • AAC
    D
  • Quantity per pack
    1
  • Unit of Measure
    Lb
  • Shelf Life
    N/A
  • Classification Control
    U
  • MGMT_CTL
    1hl1005
  • Repariability
    Medium demand velocity items (consumables)

Questions & Answers:

What are the historical prices recorded for this stock number?
Historical data shows pricing from $60.75 to $101.25..
Does NSN 3439-00-201-9119 have a shelf life?
No. There is no shelf life applicable for this NSN.
What NATO entities are users of this NSN?
Department Of The Navy
What is the NIIN of NSN 3439-00-201-9119?
002019119 or 00-201-9119
Does NSN 3439-00-201-9119 require demilitarization?
Yes - ITAR Controlled
What is the most recent solicitation for NSN 3439-00-201-9119?
No solicitations for this NSN.
When was this national stock number assigned to the federal catalog?
Apr 06, 1973
MSDS

Material Safety

MSDS BZSTF BARE-WIRE FILLER METALS, 308

Hazards

Ld50 lc50 mixture: none specified by manufacturer.

routes of entry: inhalation: yes skin: yes ingestion: no
reports of carcinogenicity: ntp: yes iarc: yes osha: no
health hazards acute and chronic: this prod poses no hlth haz as shipped
but may pose hlth haz during use. Elec arc welding rays can injure
eyes & burn skin. Dust, fumes & gases can be dangerous to hlth.

lung dmg may rslt from overexp . Short term expos to welding fumes,
gases or dust may rslt in discomfort such as dizz, naus, fever,
(efts of overexp)
explanation of carcinogenicity: nickel: iarc monographs on evaluation of
carcin risk of chems to man, vol 49, pg 257, 1990: group 2b. Ntp 7th
(ing 11)
effects of overexposure: hlth haz: dryness &/or irrit of nose, throat &
eyes. Skin sensitivity may also be noted. Acute expos can rslt in
same symps except to greater degree as well as watery eyes, hdch,
brthg dfclty, frequen t cough &/or chest pains. Some tox gases may
cause pulm edema, asphy & excess expos can be fatal. Chronic: may
(ing 12)
medical cond aggravated by exposure: some workers may experience
discomfort at concs below the tlv & others may be affected by
pre-existing cndtn or other occup illness because of the wide
variation in individual susceptibilities.

First Aid

First aid: in case of elec shock, turn off power prior to removal from
expos area & admin of first aid. Inhal: remove to fresh air. If
brthg is dfclt admin oxygen. If not brthg begin artf resp. If no
detectable p ulse begin external heart massage. Skin: wash affected
area w/soap & water. Eyes: flush w/lg amts of fresh water for at
least 15 min. Ingest: seek med attn. In all cases, seek med attn
for first aid.

Chemical Properties

Hcc: t6
appearance and odor: bare filler metals are solid wire.

Reactivity

Stability indicator/materials to avoid: yes
none specified by manufacturer.

stability condition to avoid: none specified by manufacturer.

hazardous decomposition products: welding & hot cutting fumes & gases
cannot be classified simply. Their composition & qty are dependent
on metal (supdat)

Proper Disposal

Waste disposal methods: dispose of in full compliance with federal,
state and local regulations. Avoid inhalation and skin exposure.

disclaimer (provided with this information by the compiling agencies):
this information is formulated for use by elements of the department
of defense. the united states of america in no manner whatsoever,
expressly or implied, warrants this information to be accurate and
disclaims all liability for its use. any person utilizing this
document should seek competent professional advice to verify and
assume responsibility for the suitability of this information to their
particular situation.

Ingredients List

Ingred name: iron
cas: 7439-89-6
rtecs #: no4565500
fraction by wt: balance
osha pel: n/k
acgih tlv: n/k

ingred name: chromium (sara 313) (cercla)
cas: 7440-47-3
rtecs #: gb4200000
fraction by wt: 22%
osha pel: 1 mg/m3
acgih tlv: 0.5 mg/m3
epa rpt qty: 1 lb
dot rpt qty: 1 lb

ingred name: manganese (sara 313)
cas: 7439-96-5
rtecs #: oo9275000
fraction by wt: 2.5%
osha pel: 5 mg/m3 dust, c
acgih tlv: 5 mg/m3 dust

ingred name: nickel (sara 313) (cercla)
cas: 7440-02-0
rtecs #: qr5950000
fraction by wt: 11%
osha pel: 1 mg/m3
acgih tlv: 1 mg/m3

ingred name: supdat: metallics. Gaseous rxn prods may incl carbon
monoxide, ozone & nitrogen oxides. Chlorinated solvs may be (ing 6)
rtecs #: 9999999zz

ingred name: ing 5: decomposed into tox gases such as phosgene. When
electrodes are consumed, fume & gas decomp prods generated(ing 7)
rtecs #: 9999999zz

ingred name: ing 6: are different in form from listed ingreds. New cmpds
not in electrodes may form. Known gases & fumes that (ing 8)
rtecs #: 9999999zz

ingred name: ing 7: may form during welding/hot cutting are: aluminum
fumes, carbon monoxide, chromium, chromium (chromates), (ing 9)
rtecs #: 9999999zz

ingred name: ing 8: cobalt fume, copper fume, iron oxide fume, manganese
fume, molybdenum (soluble), nickel (soluble), (ing 10)
rtecs #: 9999999zz

ingred name: ing 9: tungsten (soluble), nitrogen dioxide, ozone,
phosgene.

rtecs #: 9999999zz

ingred name: explan of carcin: annual report on carcins, 1994: antic to
be carcin. Human: lungs, nasal cavities.

rtecs #: 9999999zz

ingred name: efts of overexp: rslt in neurological dmg, lung fibrosis,
pneumoconiosis & other lung diseases. Chromium is (ing 13)
rtecs #: 9999999zz

ingred name: ing 12: considered poss carcin under osha (29cfr
1910.1200). Studies forming basis for this classification were (ing
14)
rtecs #: 9999999zz

ingred name: ing 13: from operations other than welding. There is
considerable controversy on extent of resp cancer probs. (ing 15)
rtecs #: 9999999zz

ingred name: ing 14: nevertheless, exposure must be maintained below the
specified levels.

rtecs #: 9999999zz

ingred name: resp prot: &/or worker's breathing zone to determine if
resp is reqd & type needed. Use only niosh/msha apprvd resps.

rtecs #: 9999999zz

ingred name: vent: area. Keep exposure below limits specified.

rtecs #: 9999999zz

ingred name: eye prot: & full length faceshield with filter lens.

select welding lens shade from aws publication f2.2.

rtecs #: 9999999zz

ingred name: other prot equip: welding. Do not expose skin to radia when
hot cutting/welding. Provide prot screens to shield others.

rtecs #: 9999999zz